• Cnc Chamfer End Mill Tungsten AlTiN Coating 55HRC 45HRC Endmill
  • Cnc Chamfer End Mill Tungsten AlTiN Coating 55HRC 45HRC Endmill
Cnc Chamfer End Mill Tungsten AlTiN Coating 55HRC 45HRC Endmill

Cnc Chamfer End Mill Tungsten AlTiN Coating 55HRC 45HRC Endmill

Product Details:

Place of Origin: China
Brand Name: BWIN
Model Number: D10*75-4F

Payment & Shipping Terms:

Minimum Order Quantity: 1p/box
Price: Negotiable
Packaging Details: Plastic box
Delivery Time: 7 work days
Payment Terms: T/T, Western Union
Supply Ability: 1-10000pcs 7days
Get Best Price Contact Now

Detail Information

Product Name: 45HRC 55HRC D10*75-4F Chamfer End Mill Model: D3 To D20 Chamfering Milling Cutter
Material: Tungsten Chamfering Milling Cutter Workpiece: Copper, Alloy Steel,Stainless Steel, Cast Iron
Usage: Milling Machine Coating: AlTiN
HRC: HRC45 55 Feature: Long Life
Application: Milling Machine Package: 1pcs/Box
High Light:

Chamfer End Mill 55HRC

,

Chamfer End Mill AlTiN Coating

,

AlTiN Coating Tungsten End Mill

Product Description

Cnc Tool Customized Chamfering Milling Cutter 45HRC 55HRC D10*75-4F Chamfer End Mill Endmill

Quick Detail:

  • High hardness
  • High precision
  • Good wear resistance
  • Good finish
  • Strong vibration resistance
  • Long life

Description:

  • Selected high-quality bar material, high-precision grinding process, reduce vibration, not easy to break the knife, greatly improving the service life of the knife; Unequal spiral and large chip discharge groove design enable fast chip breaking and chip discharge performance, smooth cutting, reduce burrs and not easy to stick the cutter, and achieve high productivity in cutting; High quality coating technology, different series of different coatings, easy to distinguish; Universal chamfered round handle design, easy to use, with good compatibility.

Specifications

Item Grade

 

HRC45
(YG10X )
HRC55
(YL10.2 & WF25)
HRC60
(Germany K44 &K40)
HRC65
(Sandvik H10F)

 

Details
Grain size 0.7um
Co10%
Flexural strength
3320N/mm2
Grain size 0.6um
Co10%
Flexural strength 4000N/mm2
Grain size 0.5um
Co12%
Flexural strength
4300N/mm2
Grain size 0.5um
Co10%
Flexural strength 4300N/mm2

 

Coating Classifying and Advantage
Item
Coating Type
AlTin
TiAlN
TiSiN
Naco
 
 
 
 
 
 
 
 
 
 
 
 
 
Characteristic
Hardness(HV)
3300
2800
4300
42(GPA)
Thickness(UM)
2.5-3
2.5-3
3
3
Oxidation Temp.(°C)
900
800
1000
1200
Friction Coefficient
0.35
0.3
0.25
0.4
Color
Black
Bronze
Bronze and gold
Blue
Advantages
High heat stability
Normally cutting
Suitable for heavy cutting, and high hardness cutting
For high precision cutting
Suitable for high speed, dry cutting
Suitable for cutting mould steel, stainless
steel
Suitable for high hardness cutting, mould steel processing
Most suitable for carbide cutting tools, turning insert
 
 
Cnc Tool Customized Chamfering Milling Cutter 45HRC 55HRC D10*75-4F Chamfer End Mill Endmill
Specification Flute Dia(φ) Flute Length (C) Shank Dia(D) Overall Length(L)
Φ4x10Cx4x50L 4 10 4 50
Φ5x13Cx5x50L 5 13 5 50
Φ6x15Cx6x50L 6 15 6 50
Φ8x20Cx8x60L 8 20 8 60
Φ10x25Cx10x75L 10 25 10 75
Φ12x30Cx12x75L 12 30 12 75
Φ8x35Cx8x100L 8 20 8 100
Φ10x40Cx10x100L 10 20 10 100
Φ12x45Cx12x100L 12 25 12 100
Φ14x45Cx14x100L 14 25 14 100
Φ16x45Cx16x100L 16 30 16 100
Φ18x45Cx18x100L 18 40 18 100
Φ20x45Cx20x100L 20 45 20 100

 

Tips:
  • The above specifications are standard Size, with a large amount of stock. At the same time, we support OEM customized production, the diameter is 0.2mm to 25mm, the Total length is 50mm to 200mm, include inch size end mill , the number of Flute is 4F, 5F, 6F, 8F and the logo could becustomized.
Cnc Tool Customized Chamfering Milling Cutter 45HRC 55HRC D10*75-4F Chamfer End Mill Endmill
 
Notice:
  • Handle with care to avoid impact damage.
  • The loading and unloading of milling cutter should be protected with a rag to prevent hands from being injured or the cutter edge from being damaged by falling
  • During milling, the milling cutter shall be fully separated from the working object before starting the machine to avoid damaging the cutter due to impacting the working object
  • The shorter the distance between the edge of the milling cutter and the bobbin, the better to reduce the vibration of the milling cutter. The length of the cutter should not be too long
  • Select the correct and appropriate end milling cutter to mill the working object, and select the cutting speed and feed according to the material of the working object
  • When the cutting data is unclear, the feed rate (feed rate) shall be reduced for testing, and then the processing data shall be gradually corrected to achieve the ideal production effect. Do not make rapid advances to cause damage or injury to the milling cutter.

Applications:

Pre-hardened Steel, stainless steel, Die steel, steel plate, Heat-resistant steel,pipe, copper and aluminum, cast iron, Nonferrous Metal, Wood, Plastic,FRP and sO on. General-purpose operation slotting, rilling, profiling.

Cnc Tool Customized Chamfering Milling Cutter 45HRC 55HRC D10*75-4F Chamfer End Mill Endmill

 

FAQ
1. Flank Wear? Higher cutting resistance,Notch wear on flank,Poor roughness of surface, or deterioration of accuracy.
Soft grades,Excessive cutting speed,Small flank angle,Low feed.
Select a higher,wear-resistant grade,Reduce cutting speed,Increase flank angle,Increase feed.
 
2. Crater Wear? Uncontrolled chip,Poor surface quality,when finishing High speed processing carbon steel
Soft grades,Excessive cutting speed,Excessive feed,The strength of chip breaker Insufficiet.
Change to a higher wear-resistant grade,Reduce cutting speed,Reduce feed,Select a higher strength chip breaker.
 
3. Chipping? Sudden fracture of cutting edge(rake face and flank),Instability insert life
Toughness insufficient,Excessive feed rate,Strength of cutting edge insufficient,Instability of the tool.
Select a tougher grade,Decrease feed rate,Increase honing of cutting edge(chamfering to rounding),Increase the stability and setting angle
 
4. Insert Fracture? Cutting resistance increased Poor surface roughness.
Toughness insufficient,Excessive feed rate,Strength of cutting edge insufficient,Instability of the tool.
Select a tougher grade,Decrease feed rate,Increase honing of cutting edge(chamfering to rounding),Increase the stability and setting angle.
 
5. Plastic Deformation? Variation of dimension Nose wear,cutting edge drape or passivating.when processing alloy steel Poor surface roughness
Soft grade,Excessive cutting speed,Excessive cutting depth and feed rate,Overheat on cutting edge.
Select a higher red hardness cutting material,Decrease cutting speed,Decrease cutting depth and feed rate,Select a higher thermal conductivity cutting material(CVD+sufficient coolant).
 
6. Build-Up-Edge? Workpiece dissove with Cutting edge Poor surface roughness when finishing,Cutting resistance increased,Cutting soft materials.
Cutting speed too low,Cutting edge obtuse,Unsuitable tool material. Increase cutting speed,Increase rake angle,Select small sticking force.

 