Scgt 09t302 CNC Carbide Inserts Aluminum Lathe Turning Insert High Durability
Product Details:
Place of Origin: | China |
Brand Name: | BWIN |
Model Number: | Scgt120408 |
Payment & Shipping Terms:
Minimum Order Quantity: | 10pcs/box |
---|---|
Price: | Negotiable |
Packaging Details: | Plastic box |
Delivery Time: | 7 work days |
Payment Terms: | T/T, Western Union |
Supply Ability: | 1-10000pcs 7days |
Detail Information |
|||
Product Name: | Scgt CNC Carbide Turning Insert | Material: | Tungsten Lathe Turning Insert |
---|---|---|---|
Workpiece: | Aluminum | Usage: | CNC Lathe |
Color: | Uncoated | Coating: | PVD CVD |
Hardness: | HRC40-60 | Feature: | Smooth Cutting |
Application: | CNC Tool | Package: | 10pcs/Box |
Highlight: | Scgt 09t302 CNC Carbide Inserts,Lathe Turning Insert Scgt 09t302,Lathe Turning Insert High Durability |
Product Description
Cnc Carbide Turning Insert Scgt 09t302 09t304 120402 120404 120408 120412 Lathe Aluminum
Quick Detail:
- Good red hardness
- Smooth chip removal
- High production efficiency
- Good heat dissipation condition
- High durability
Description:
- SCGT cnc carbide inserts are sintered from tungsten carbide and cobalt powder. The base material with strong deformation resistance and carbide with special crystal structure enable the tool to have high hardness, good toughness and high temperature resistance, making the wear resistance of the rear face of the tool stronger; Sharp edge, sturdy and durable, full edge anti-seismic design can restrain chatter during processing, and improve the surface finish; Complete specifications to meet your different processing needs.
Specifications:
Brand | BWIN |
Model | CNMG120404 CNMG120408 CNMG120412 |
Color | Yellow/Brown/Fuchsia/Black/cermet/Uncoated |
Workpiece | Cast iron/Steel/Stainless steel/Aluminium |
Type | CNC Carbide Insert |
Material | Tungsten Carbide Turning Insert |
Processing Type | Medium Cutting |
Feature | Good red hardness |
Smooth chip removal | |
High strength | |
Good heat dissipation condition | |
High durability |
|
Standard | ISO |
Quantity | 10pcs/box |
Weight | 0.015kg |
Package | Plastic Box |
Customized Support | OEM, ODM |
Lead Time:
antity(pieces) | 1 - 3000 | >3000 |
Lead time (days) | 7 | To be negotiated |
I(mm)
|
d(mm)
|
t(mm)
|
d1(mm)
|
09
|
9.525
|
3.97
|
4.4
|
12
|
12.7
|
4.76
|
5.5
|
Notice:
- The cnc carbide inserts shall not be collided or dropped on the ground and must be handled with care.
- Before installing the cnc carbide inserts, the performance and purpose of the saw table must be confirmed to ensure that the cutting direction indicated by the blade arrow is consistent with the rotation direction of the saw table. It is strictly prohibited to install in the opposite direction. Wrong installation direction may cause the blade sawtooth to fall off, so as to prevent accidents.
- After installation, it is necessary to confirm whether the central hole of the cnc carbide inserts are firmly fixed on the flange plate of the saw table. If there is a gasket, the gasket must be sleeved; Then, gently push with your hand to confirm whether the blade rotates eccentrically.
- When using, do not exceed the specified high speed
- When the cnc carbide inserts are not used, hang the blade vertically on the dry shelf.
Applications:
Our cnc carbide inserts could to be processed Alloy steel, Tool steel, carbon steel, stainless steel, Cast iron and Titanium alloy. Working material as following:
FAQ
1. Flank Wear? Higher cutting resistance,Notch wear on flank,Poor roughness of surface, or deterioration of accuracy.
Soft grades,Excessive cutting speed,Small flank angle,Low feed.
Select a higher,wear-resistant grade,Reduce cutting speed,Increase flank angle,Increase feed.
2. Crater Wear? Uncontrolled chip,Poor surface quality,when finishing High speed processing carbon steel
Soft grades,Excessive cutting speed,Excessive feed,The strength of chip breaker Insufficiet.
Change to a higher wear-resistant grade,Reduce cutting speed,Reduce feed,Select a higher strength chip breaker.
3. Chipping? Sudden fracture of cutting edge(rake face and flank),Instability insert life
Toughness insufficient,Excessive feed rate,Strength of cutting edge insufficient,Instability of the tool.
Select a tougher grade,Decrease feed rate,Increase honing of cutting edge(chamfering to rounding),Increase the stability and setting angle
4. Insert Fracture? Cutting resistance increased Poor surface roughness.
Toughness insufficient,Excessive feed rate,Strength of cutting edge insufficient,Instability of the tool.
Select a tougher grade,Decrease feed rate,Increase honing of cutting edge(chamfering to rounding),Increase the stability and setting angle.
5. Plastic Deformation? Variation of dimension Nose wear,cutting edge drape or passivating.when processing alloy steel Poor surface roughness
Soft grade,Excessive cutting speed,Excessive cutting depth and feed rate,Overheat on cutting edge.
Select a higher red hardness cutting material,Decrease cutting speed,Decrease cutting depth and feed rate,Select a higher thermal conductivity cutting material(CVD+sufficient coolant).
6. Build-Up-Edge? Workpiece dissove with Cutting edge Poor surface roughness when finishing,Cutting resistance increased,Cutting soft materials.
Cutting speed too low,Cutting edge obtuse,Unsuitable tool material. Increase cutting speed,Increase rake angle,Select small sticking force.